Analisis Korosifitas Baja Ringan dengan Metoda Laser Induced Breakdown Spectroscopy (LIBS)

Authors

  • Siti Raudatul Jannah Prodi Studi Fisika, FMIPA, Universitas Udayana
  • Ni Nyoman Ratini Prodi Studi Fisika, FMIPA, Universitas Udayana
  • Windarjoto Windarjoto Prodi Studi Fisika, FMIPA, Universitas Udayana
  • Hery Suyanto Prodi Studi Fisika, FMIPA, Universitas Udayana

DOI:

https://doi.org/10.29408/kpj.v5i1.3446

Keywords:

Mild steel, NaCl, Element identification, Corrosion rate

Abstract

Method has been carried out. Research is done on mild steel zincalume type with immersion treatment (NaCl 3.5%) for 10 days, and 30 days and without immersion. Mild steel is laser irradiated (Nd-YAG 1064 nm, 7 ns) with energy of 120 mJ, and the data is taken with an accumulation of 3, delay time of 0.5 µs. Elements identification is done by taking data from up to 75 μm from the surface. The results of the analysis with LIBS showed immersion for 10 days, the corrosion rate and hardness of mild steel increased with 30 days immersion. The increase in the corrosion rate of mild steel is indicated by decreasing the value of dissolved oxygen intensity, the electrochemical reaction is fast. The decrease in the corrosion rate is indicated by the increase in the intensity value of Zn and Al elements associated with the formation of a passive film on the metal surface as a protective layer to protect further corrosion attacks.


DOI : 10.29408/kpj.v5i1.3446

References

Anissa, F. D. Y. (2016) Pengaruh pH Air Hujan dan Beban Terhadap Karakteristik Korosi pada Baja Galvalum, Surabaya: Institut Teknologi Sepuluh Nopember.

Agus, S. (2014) Perencanaan Rangka Atap Baja Ringan, TAPAK, Dosen Fakultas Teknik Universitas Muhammadiyah Metro, vol. 3, no. 2, pp. 91-95.

Arga, J. S., Sutan, L. M. H. S., & Charles, S. P. M. (2020) Analisa Laju Korosi dan Kekerasan Pada Stainless Steel 316 L Dalam Larutan 10% NaCl Dengan Variasi Waktu Perendaman, SjoME, vol.1, no. 2, pp. 92-99.

Fajar, N. (2014) Baja Ringan sebagai Salah Satu Alternatif Pengganti Kayu pada Struktur Rangka Kuda-Kuda Ditinjau dari Segi Konstruksi. Jurnal Momentum, vol. 16, no. 2, pp. 108-118.

Gadang, P., Siska, P., Lutviasari, N., Sundjono., Ibrahim, P. (2019) Korosi Baja di Muara Jakarta dan Indramayu dengan Simulasi Pasang Surut Uji Wet Dry, Jurnal Kelautan, vol. 12, no. 01, pp. 23-35.

Hakim, D. (2016) Efektifitas Penggunaan Baja Ringan untuk Struktur Rangka Atap Gedung, Jurnal Ilmiah Teknik Tekstur Kota, vol. VII, No.2, Fakultas Teknik Jurusan Arsitektur, Universitas Pepabri Makassar; pp. 79-88.

Andreas, S. I., & Radhian, K. (2015) Ketahanan Korosi Baja Ringan di Lingkungan Air Laut, Jurnal Material dan Teknologi Proses, vol. 1, no. 1, pp. 1-7.

Hery, S. (2013) Identifikasi Unsur Utama Penyusun Permukaan Bahan Baja Ringan dengan Laser Induced Breakdown Spectroscopy (LIBS), Jurnal Energi dan Manufaktur, vol. 6, no. 2, pp. 151-156.

Hery, S., Ni, L. P. Trisnawati., I, K. Putra., & Iryanti, S. (2018) Characterization of Human Teeth by Laser Induced Breakdown Spectroscopy (LIBS), Journal of Physics Conference Series, pp. 1-6.

Muhammad, Z. (2017) Analisis Laju Korosi dengan Penambahan Pompa pada Baja Komersil dalam Media Air Laut, Jurnal Mekanikal, vol. 8, no. 2,pp. 737-741.

Nasrullah, Idris., Tjoet, N. U., Herman., & M, R. (2018) Karakteristik Fisik Plasma dalam Laser Induced Breakdown Spectroscopy (LIBS) Menggunakan Laser Neodymium: Yttrium-Aluminium-Garnet (Nd-YAG) Pada Sampel Daging Kerang Sungai, Risalah Fisika, vol. 2, no. 1, pp. 9-14.

Richard, D. P., J, Stuart. A., & John, S. C. (2015) Application of laser-induced breakdown spectroscopy for surface hardness measurements, Spectroscopyeurope, vol. 27, no. 6, pp. 13-15.

Sundjono., Gadan, P., Lutviasari, N., & Siska, P. (2017) Corrosion Behavior of Mild Steel in Seawater from Northern Coast of Java and Southern Coast of Bali, Indonesia, Journal of Engineering and Technological Sciences, pp. 770-784

Vita, R., & Muzkantari. (2015) Pengaruh Variasi TiO2 dalam Komposit PANi-TiO2/Cat sebagai Pelapis Anti Korosi pada Baja Karbon ASTM A36, Jurnal Inovasi Fisika Indonesia, vol. 4, no. 3.

Wahyu, S. B., Hery, S., Hendrik, K., May, O. T., & Kiichiro, K. (1999) Shock Excitation and Cooling Stage in the Laser Plasma Induced by a Q-Switched Nd;YAG Laser at Low Pressures, Applied Spectroscopy, vol. 53, pp. 1347-1351.

Winardi, T. B, H., & Hery, S. (2014) Analisis Signal Latar Plasma Laser dan Effeknya, dengan Laser Induced Breakdown Spectroscopy (LIBS), Simposium Fisika Nasional.

Zhang, X. (2012) The Initial release of zinc and aluminium from non-treated Galvalume and the formation of corrosion products in chloride containing media, Swedia: Science Direct.

Zienab, A. S., Z, Nanjing., D, Anglos., & M, Abdel. H. (2009) Effect of experimental conditions on surface hardness measurements of calcified tissues via LIBS, Applied Physics B, pp. 141-147.

Downloads

Published

2021-06-30

Issue

Section

Articles